Charge carrier density, mobility, and Seebeck coefficient of melt-grown bulk ZnGa2O4 single crystals
The temperature dependence of the charge carrier density, mobility, and Seebeck coefficient of melt-grown, bulk ZnGa2O4 single crystals was measured between 10 K and 310 K. The electrical conductivity at room temperature is about σ = 286 S/cm due to a high electron concentration of n = 3.26 × 1019 c...