Effect of Normalizing and Annealing Process on High Frequency Magnetic Properties and Strength of Cold-Rolled Non-Oriented Silicon Steel
The cold-rolled non-oriented silicon steel (/%: 0.003C, 2.35Si, 0.22Mn, 0.011P, 0,002S, 0. 36Al, 0.003 0N) is cold-rolled to 0.35 mm sheet from 2. 3 mm hot-rolled plate normalized at 890 °C or 940 for 3 min. The effect of normalizing temperature and annealing process at 800 ~ 920 ℃ for 3 min on high...