QR Code (код быстрого отклика)

Acid-resistant clay bricks incorporating bottom ash and waste glass strengthened by mullite suppression and albite formation

This study reports a systematic investigation of vitrification-driven modification of fired clay ceramics through the co-utilization of lignite-derived bottom ash (BA) and post-consumer waste glass (WG). Clay bodies containing 2.5–10.0 wt% BA–WG (1:1 mass ratio) were fired at 900–1100 °C to evaluate...

Полное описание

Сохранить в:
Библиографические подробности
Главные авторы: Siwat Lawanwadeekul, Prinya Chindaprasirt, Nattawut Ariyajinno, Anuwat Srisuwan, Nonthaphong Phonphuak
Формат: Artigo
Язык:Inglês
Опубликовано: Elsevier 2026-04-01
Серии:Next Materials
Предметы:
Online-ссылка:http://www.sciencedirect.com/science/article/pii/S2949822826000274