Código QR (código de barras bidimensional)

Effect of cooling rates on T6 Treatment of B390 Aluminium-Silicon Hypereutectic alloys

This research aimed to study an effect of cooling rates on T6 treatment process of B390 aluminium hypereutectic alloy. B390 casting samples were casted with pouring temperature of 710°C and solidified in three different cooling rates of 33.33, 28.60 and 22.22°C/s, respectively using three metal moul...

ver descrição completa

Na minha lista:
Detalhes bibliográficos
Principais autores: Jiandon Porawit, Talangkun Sukangkana
Formato: Artigo
Idioma:Inglês
Publicado em: EDP Sciences 2019-01-01
coleção:MATEC Web of Conferences
Acesso em linha:https://www.matec-conferences.org/articles/matecconf/pdf/2019/42/matecconf_acmme2019_02001.pdf