Microstructure and Shear Strength of SiC Joint Brazed with LiAlSiO<sub>4</sub> Reinforced AgCuTi Composite Filler
In this work, SiC ceramics were successfully brazed at 900 °C using a composite brazing filler, and the effects of holding time and LiAlSiO<sub>4</sub> addition on the interfacial microstructure and mechanical properties of the joints were systematically investigated. The results showed that the bra...