Effects of Pre-Strain on the Evolution of Microstructure and Strain Hardening of Extruded Az31 Magnesium Alloy
Pre-compression 3% and pre-stretch 3% subsequent annealing at 200ºC for 2h are conducted on AZ31 magnesium alloys, then inverse tensile and compressive deformation are carried out at room temperature, respectively. During inverse tension 3% deformation on 1st pre-compression samples, detwinning beha...