Effect of annealing temperature on microstructure and mechanical property of Ti-0.3Mo-0.8Ni-0.01Y alloy

In this study, a novel near-α titanium alloy, Ti-0.3Mo-0.8Ni-0.01Y (TA10-0.01Y wt.%), was fabricated using a vacuum non-consumable arc-melting furnace. The effects of annealing temperature (670 °C, 770 °C, and 870 °C) on the microstructure and mechanical properties of TA10-0.01Y plates were systemat...