Influence of Post-Curing Time and Print Orientation on the Mechanical Behavior of Photosensitive Resins in mSLA 3D Printing

This study investigates the mechanical behavior of water-washable photosensitive resins used in masked stereolithography (mSLA) 3D printing, evaluating the effect of post-curing time (0, 5, 10, 30, and 60 min) and printing orientation (Flat [XY], Vertical [Z], and On-edge [XZ]) on the material chara...