Simultaneously high-energy storage density and responsivity in quasi-hysteresis-free Mn-doped Bi0.5Na0.5TiO3-BaTiO3-(Sr0.7Bi0.2□0.1)TiO3 ergodic relaxor ceramics
High-energy storage density, responsivity and efficiency, i.e. WR = 1.07 J/cm3, ξ = 119 J/(kV m2) and η = 92%, were simultaneously obtained in Mn-doped 0.62Bi0.5Na0.5TiO3-0.06BaTiO3-0.32(Sr0.7Bi0.2□0.1)TiO3 ergodic relaxor ceramics. Appropriate Mn doping was beneficial to enhance breakdown field str...