Effect of Calcium and Boron on Structure and Magnetic Properties of Non-Oriented Silicon Steel
The 3 kinds of non-oriented silicon steel (/% : 0.004-0.006C, 1.31-1.38Si, 0.34-0.41Mn, 0.004S, 0.027P, 0.36-0.41Als, 0.0022-0.0028 T[O], 0.0048-0.0060N) - non containing Ca and B, containing Ca (0.0026% Ca) , and containing Ca-B (0.0027% Ca and 0.0045% B) is melted by a 6.5 kg vacuum induction furn...