Studying the optical properties of tZnxCd1 – x S thin films prepared by chemical bath deposition (CBD) and the effect of annealing temperature.

The ZnxCd1 – x S (x=0.2,0.5,0.7) thin films have been deposited by chemical both deposition method on glass substrates from aqueous solution containing cadmium acetate , zincacetate and thiourea at 80±5 ℃and after annealed at 150-200 ℃. optical method was used to determine the band gap of films betw...