Effect of casting speed rising on the cleanliness of IF steel slab during the initial casting stage

During the initial casting stage of the IF steel, the cleanliness of the first slab deteriorates. Steel plants treat the initial casting slabs as waste or demoting products. Moreover, the cleanliness deterioration of initial casting slabs leads to unstable quality and low product yield. In the prese...