VERTICAL CENTRIFUGAL CASTING OF A HYPEREUTECTIC SILUMIN WITH COOLING OF THE MOLD AND CASTING
It is shown that cooling of casting molds by water with water flow of 0,42 m3/h and internal surfaces of castings with thickness of a wall 12–14 mm with water quantity 2,5×10–4–5×10–4 m3 allows to receive procurements with completely modified microstructure without use of modifiers. External layers...
Сохранить в:
| Главные авторы: | , , |
|---|---|
| Формат: | Artigo |
| Язык: | Inglês |
| Опубликовано: |
Belarusian National Technical University
2017-07-01
|
| Серии: | Литьë и металлургия |
| Предметы: | |
| Online-ссылка: | https://lim.bntu.by/jour/article/view/1982 |
| Метки: |
Нет меток, Требуется 1-ая метка записи!
|