QR Code

Ablation properties of ZrC-SiC-HfB2 ceramic with different amount of carbon fiber under an oxyacetylene flame

In the present work, a carbon fiber reinforced ZrC-20 vol% SiC-15 vol% HfB _2 composite was produced by pressureless sintering method. Carbon fiber with various weight percentages (0, 10, 20, 30) was added to the milled ZrC-SiC-HfB _2 . The mixed powders were pressed and sintered at 2200 °C for 2 h....