Increasing Continuous - Continuous Casting Success Rate of Steel 38CrMoAl by Optimizing Deoxidation Process

The types and formation cause of inclusions in casting steel 38CrMoAl (/%: 0. 35 ~ 0. 42C, 0. 20 ~0. 45Si, 0. 30 - 0. 60Mn, 1. 35 〜1.65Cr, 0. 15 ~ 0. 25Mo, 0. 70 - 1. 10A1) are studied. By optimizing deoxidation technique including increasing 60 t EAF end [C] ≥ 0. 010% and maintaining high basicity...