Analysis and Process Improvement of Hot Bending Cracking of SA-106B Seamless Steel Pipe

After induction heating, the SA-106B seamless steel pipe has cracks during hot bending process, the physical and chemical properties of the SA-106B seamless steel pipe and the hardness uniformity of the full cross-section were analyzed, and the cracking samples were tested by optical microscope. Com...