Corrosion Resistance of SiO<sub>2</sub> Aerogel Loaded with Benzotriazole Inhibitor in K<sub>2</sub>SiO<sub>3</sub> Coatings
In order to enhance the corrosion protection of K2SiO3 coatings, SiO2 aerogel (SA) was used as a carrier loaded with 70 mg/mL benzotriazole (BTA) corrosion inhibitor (SA@BTA-70).The SA@BTA-70 dispersion and BTA slow-release properties in K2SiO3 solution were researched,and their...
Tallennettuna:
| Päätekijä: | |
|---|---|
| Aineistotyyppi: | Artigo |
| Kieli: | Chinês |
| Julkaistu: |
Editorial Department of Materials Protection
2024-09-01
|
| Sarja: | Cailiao Baohu |
| Aiheet: | |
| Linkit: | http://www.mat-pro.com/fileup/1001-1560/PDF/20240907.pdf |
| Tagit: |
Ei tageja, Lisää ensimmäinen tagi!
|