BOROSILICATE GLASS FOAM EXPERIMENTALLY MANUFACTURED BY MICROWAVE IRRADIATION

A glass foam obtained by sintering at 790 ºC using borosilicate glass waste, carbon black (1%) as a foaming agent, Na2HPO4 (5.9%) as a stabilizing agent, Sb2O3 (0.8%) as an oxygen supplying agent and water addition (10%) as a binder was manufactured by microwave irradiation. The glass foam characte...