QR kód

Erosion wear performance of HVOF sprayed WC-10Co-4Cr + 2% TiO2 coating on SS-409 using slurry jet erosion tester

Erosion is a phenomenon and is the primary cause of failure in numerous slurry transportation equipment such as pump impellers, pipeline fittings, etc. It reduces the working life of the equipment and is thus an essential factor in the design, choice, and operation of any system. Pipeline materials...

Celý popis

Uloženo v:
Podrobná bibliografie
Hlavní autoři: Asisha Ranjan Pradhan, Satish Kumar, Chandan Gupta, Swaroop Kumar Mandal
Médium: Artigo
Jazyk:Inglês
Vydáno: Elsevier 2024-08-01
Edice:Results in Surfaces and Interfaces
Témata:
On-line přístup:http://www.sciencedirect.com/science/article/pii/S2666845924000977