Mechanical Behavior and Microstructure Evolution of a Ti-15Mo/TiB Titanium–Matrix Composite during Hot Deformation

A Ti-15Mo/TiB titanium&#8722;matrix composite (TMC) was produced by spark plasma sintering at 1400 &#176;C under a load of 40 MPa for 15 min using a Ti-14.25(wt.)%Mo-5(wt.)%TiB<sub>2</sub> powder mixture. Microstructure evolution and mechanical behavior of the composite were studied during uniaxial...