Novel process for the production of 3Y-TZP ceramics: comparison between ageing in artificial saliva and accelerated ageing
The degradation of tetragonal zirconia polycrystalline (3Y-TZP) ceramics prepared by a novel film growth technique, and by sintering at 1400 °C, was evaluated for one year using two processes: (i) degradation under oral conditions in artificial saliva (37 °C and pH 6.8) and (ii) accelerated degradat...