NIOBIUM EFFECT ON BASE METAL AND HEAT AFFECTED ZONE MICROSTRUCTURE OF GIRTH WELDED JOINTS
The development of steels for line pipes during the last decades has been driven by the need to obtain improved combinations of high strength, toughness, weldability on industrial scale at affordable prices. The effect of niobium content on the heat affected zone (HAZ) microstructure is reported in...