Fabrication and Electrical Characterization of Translucent Bi12TiO20 Ceramics
The production of high-density Bi12TiO20 ceramics, their transmission spectrum, and impedance features are reported. The samples were synthesized at 700°C/6 h and sintered at 800°C/3 h. This procedure yielded translucent ceramics with relative density of 99.2±0.5% and average grain size of 3.1±1.6 μ...