Effect of Process Variables on Friction Stirred Microstructure and Surface Hardness of AZ31 Magnesium Alloy

Effects of various friction stir processing (FSP) variables on the microstructural evolution and microhardness of the AZ31 magnesium alloy were investigated. The processing variables include rotational and travelling speed of the tool, kind of second phase (i.e., diamond, Al2O3, and ZrO2) and groove...