The growth of Nd:CaWO4 single crystals
CaWO4 doped with 0.8 % at. Nd (Nd:CaWO4) single crystals were grown from the melt in air by the Czochralski technique. The critical diameter dc = 1.0 cm and the critical rate of rotation ωc = 30 rpm were calculated from hydrodynamic equations for buoyancy-driven and forced convection. The rate of cr...