Investigating the Role of Hydrofluoric Acid Concentration in Tailoring the Morphology and Enhancing the Photonic Properties of Nanoporous Silicon Wafers
At This research used an electrochemical method to convert bulk silicon wafers into porous silicon (PS). The wafers, chosen with a (100) orientation and (8-3) Ω.cm resistivity, the time of etching was 25 min and the current density of etching 25 mA/cm². It was carried out nanoscale surface morpho...
שמור ב:
| מחבר ראשי: | |
|---|---|
| פורמט: | Artigo |
| שפה: | Inglês |
| יצא לאור: |
Tikrit University
2024-12-01
|
| סדרה: | Tikrit Journal of Pure Science |
| נושאים: | |
| גישה מקוונת: | https://tjpsj.org/index.php/tjps/article/view/1718 |
| תגים: |
אין תגיות, היה/י הראשונ/ה לתייג את הרשומה!
|