Study on edge effects in salt frost scaling tests: Implications for surface degradation assessment

Surface scaling and internal structural deterioration caused by cyclic freezing and thawing exposure are among the most common degradation mechanisms in concrete structures exposed to cold climates. Standard laboratory methods such as the CDF (Capillary suction of Deicing Chemicals and Freeze-thaw)...