Crystal structure and piezoelectric properties of 0.79(Na0.5Bi0.5)TiO3-0.05BaTiO3-0.16(K0.5Bi0.5)TiO3 ceramics prepared by solid–state method

The solid-state reaction technique was employed to synthesize lead-free ceramics, specifically (1-x-y)(Na0.5Bi0.5)TiO3-xBaTiO3-y(K0.5Bi0.5)TiO3. For attaining a pure perovskite phase, it was found that the optimal calcination temperature is 1000 °C, maintained for a duration of 4 h. Through X-ray di...

Бүрэн тодорхойлолт

-д хадгалсан:
Номзүйн дэлгэрэнгүй
Үндсэн зохиолчид: M. Mesrar, T. Lamcharfi, N.-S. Echatoui, F. Abdi
Формат: Artigo
Хэл сонгох:Inglês
Хэвлэсэн: Elsevier 2024-06-01
Цуврал:Heliyon
Нөхцлүүд:
Онлайн хандалт:http://www.sciencedirect.com/science/article/pii/S2405844024092983