Effects of Sintering Processes on Microstructure Evolution, Crystallite, and Grain Growth of MoO<sub>2</sub> Powder
MoO<sub>2</sub> micro-powders with a mean pore size of 3.4 nm and specific surface area of 2.5 g/cm<sup>3</sup> were compacted by dry pressing, then pressureless sintered at a temperature of 1000–1150 °C for 2 h or for a sintering time of 0.5–12 h at 1050 °C in an N<sub>2</sub> atmosphere. Then, the...