Analysis of initial crack path in fretting fatigue

The initial crack path is analysed in a fretting fatigue test with cylindrical contact, where there is a stress gradient and a multiaxial and non-proportional stress state. For this, a cylindrical pad is pressed, with a constant normal load, N, against a dog-bone type fatigue test specimen. Then, th...