The Effect of Service Conditions on the Performance of Silicone and Neoprene Elastomer Materials
In this study, the behavior of VMQ and CR materials under harsh service conditions (compression and temperature) were investigated. For this purpose, a group of samples were compressed at a rate of 25%, and then they were subjected to a temperature treatment between 293 K and 373 K for 24 hours. Aft...