Effect of Ce addition on hot deformation behavior and microstructure evolution of AZ80 magnesium alloy
Hot compression tests of AZ80 and AZ80-Ce alloys were conducted on a Gleeble-3800 simulator at strain rates of 0.01–10 s−1 and deformation temperatures of 340–420 °C. The effects of Ce addition on hot deformation behavior and microstructure evolution of AZ80 magnesium alloys were investigated. The r...