QR Kod

Effect of SPS Sintering Temperature on Properties of ZrB<sub>2</sub>-SiC Ceramic

Two ZrB<sub>2</sub>-20<private-char description="%">%</private-char> (volume fraction) SiC(ZS) ceramics were sintered successfully by spark plasma sintering (SPS) process at 1700 ℃ and 1900 ℃ respectively. The SEM, EDS, hardness, fracture toughness, bending strength, mass gain and cross section of o...

Ful tanımlama

Kaydedildi:
Detaylı Bibliyografya
Asıl Yazarlar: LI Qi, GUO Fengwei, CAO Lamei, YI Xiaosu
Materyal Türü: Artigo
Dil:Chinês
Baskı/Yayın Bilgisi: Journal of Aeronautical Materials 2018-08-01
Seri Bilgileri:Journal of Aeronautical Materials
Konular:
Online Erişim:http://jam.biam.ac.cn/CN/Y2018/V38/I4/87