Effect of Post-Oxidation on SnO2 Thin Films
An investigation which include synthesis of SnO2 thin film by depositing onto glass substrates at room temperature using thermal evaporation technique. The films were post-annealing in furnace tube at 250 oC temperature for different time (10, 20, 30 and 40 minutes). The films were characterized by...