Damage characterization of GFRP composite on exposure to cyclic loading by acoustic emission

Cross ply (0/90/90/0) and angle ply (0/30/60/0) glass fibre reinforced epoxy (GFRP) composite laminates were exposed to constant amplitude cyclic loading at 8.6 Hz with varying load cycles. The load is imposed on the specimen to simulate the load (considering road tyre interaction) on a leaf of auto...

Täydet tiedot

Tallennettuna:
Bibliografiset tiedot
Päätekijät: Loganathan T.G., Murthy Krishna R., Chandrasekaran K.
Aineistotyyppi: Artigo
Kieli:Inglês
Julkaistu: University of Belgrade - Faculty of Mechanical Engineering, Belgrade 2016-01-01
Sarja:FME Transactions
Aiheet:
Linkit:https://scindeks-clanci.ceon.rs/data/pdf/1451-2092/2016/1451-20921602139L.pdf