Antimony recovery from recycled terminals of lead-acid batteries with Na2CO3 and SiC after firstly SsB2O3 formation

Terminals obtained from spent lead-acid batteries in Mexico contain around 2 wt% Sb. The terminals were melted in an electric furnace and then oxygen was injected at 750 °C with a gas flow rate of 2 L/min to produce high purity Sb2O3. The antimony trioxide obtained was treated with a mixture of Na2C...