Thickness Effects on Oxidation Behavior and Consequent γ’ Degradation of a High-Al Ni-Based Single Crystal Superalloy

High temperature oxidation is considered to play an essential role in the thickness debit effect on the creep rupture life of Ni-based single crystal (SC) superalloys. In order to clarify thickness effects, thin-walled specimens of different thickness (t = 0.1, 0.3, 1.0 mm) were prepared. Cyclic and...