The impact of submerged friction stir processing on the friction stir welded dissimilar joints

The submerged friction stir processing (SFSP) technique was employed on the prior friction stir welded (FSW) AA6082/AA8011 dissimilar aluminum alloy joints. The tap water with room temperature was kept at 40 mm depth throughout the processing. The AA6082 was kept at the advancing side during FSW and...