Shrinkage Depression Formation and Yield of Ti–48 at.% Al–2 at.% Nb–2 at.% Cr Ingots Produced by Bottom-Pouring Cold Crucible Induction Melting

In this study, a Ti–48 at.% Al–2 at.% Nb–2 at.% Cr alloy was cast by bottom-pouring cold crucible induction melting (CCIM), and the shrinkage depressions formed in ingots during solidification were investigated. Ingots with different heights were produced, and shrinkage depression height and yield w...