Investigating Nanoindentation Creep Behavior of Pulsed-TIG Welded Inconel 718 and Commercially Pure Titanium Using a Vanadium Interlayer

In a dissimilar welded joint between Ni base alloys and titanium, creep failure is a potential concern as it could threaten to undermine the integrity of the joint. In this research, the mechanical heterogeneity of a Pulsed TIG welded joint between commercially pure titanium (CpTi) and Inconel 718 (...