Analysis on Inclusions in Low Aluminium Steel 15CrMoG for Boiler Pipe Refining in 100t LF by Si-Ca Deoxidation

The production process flowsheet of steel 15CrMoG for high pressure boiler pipe (/% : 0.12~0.18C, 0.17~0.35Si, 0.40~0.70Mn, ≤0.015P, ≤0.015S, 0.80~1.lOCr, 0.40~0.55Mo, ≤0.020Alt) is 60% hot metal + quality scrap- 100t UHP EAF-LF -VD-Φ500mm bloom casting-rolling. With Al-Si pre-deoxidation in EAF tap...