Increasing of hot workability of 1.3302HIGH speed steel
Laboratory investigation of hot workability of 1.3302 high speed steel was carried out and its improving was achieved. Hot compression tests for the determination of optimal soaking temperature as well as for the study of hot workability in temperature range 1150-850 ºC, strain rates range 0,001-6 s...