Effect of Degassing Treatment on the Interfacial Reaction of Molten Aluminum and Solid Steel
The gas porosity is one of the most serious problems in the casting of aluminum. There are several degassing methods that have been studied. During smelting of aluminum, the intermetallic compound (IMC) may be formed at the interface between molten aluminum and solid steel of crucible furnace lining...