Comparison of Elastic and Corrosion Behaviour of Sintered Iron Before and After Its Long Time Immersion in Hank's Solution

Test bars were prepared from an iron powder by pressing and sintering. Sintered bars exhibited porosity between 15 and 40%. Because of their shape and volume fraction, the pores were expected to form a continuous inter-connected bar-spanning structure. Effective Young's modulus, determined from the...