Properties of natural hydroxyapatite prepared by pressureless sintering using different temperatures and holding times
The sintering behavior of hydroxyapatite (HAp) particles prepared via pressureless sintering was investigated. The powders were subjected to different sintering temperatures of 900°C and 1000°C for 2, 4, and 6 hours (hr). The sintered HAp powders were analyzed for phase stability, density, Vickers h...