Investigating hot tearing in 6xxx-series aluminium alloys: A combined thermodynamic and experimental approach

The hot tearing of 6xxx-series aluminium alloys has been investigated over four levels of silicon (0.6, 0.8, 1.0, 1.2 wt%), magnesium (0.4, 0.6, 0.8, 1.0 wt%), iron (0.2, 0.4, 0.6, 0.8 wt%) and manganese (0.0, 0.2, 0.4, 0.6 wt%). Thermodynamic calculations based on the CALPHAD method were performed...