Enhanced D retention in RAFM steel caused by D bubbles formed inside Cr-rich surface layer

To identify the cause for an enhanced D retention in RAFM (reduced-activation ferritic/martensitic) steels with decreasing incident D fluence, ϕD, CLAM steel samples were exposed to D plasma at a low ϕD ∼ 3 × 1023 m−2 in the PISCES-A linear plasma device. At this low ϕD, a Cr-rich surface layer with...