High Temperature Performance of Spark Plasma Sintered W<sub>0.5</sub>(TaTiVCr)<sub>0.5</sub> Alloy
The phase stability, compressive strength, and tribology of tungsten alloy containing low activation elements, W<sub>0.5</sub>(TaTiVCr)<sub>0.5</sub>, at elevated temperature up to 1400 °C were investigated. The spark plasma sintered W<sub>0.5</sub>(TaTiVCr)<sub>0.5</sub> alloy showed body centered...