Influence of calcination temperature on catalytic activity of nanoceria
Nanoceria was synthesized by reaction of cerium nitrate deposition in an aqueous medium without stabilizers at room temperature. Nano-sized cerium oxide was dried at 20 °C and calcinated in air for 1 hour at 120, 300, 500, 800 °C. SEM images of samples demonstrated that the morphology of the obtain...