Por Ozimina D., Madej M., Kowalczyk J.
Publicado em 2017-12-01
... were examined using a JSM-7100F SEM. The coating microhardness was measured with a Matsuzawa tester...
Obter o texto integral
Artigo
3
Por Leszczyńska-Madej B., Richert M.W., Perek-Nowak M.
Publicado em 2015-06-01
... is maintained at a similar level – equal to d = 0.55-0.59 μm. A combination of ECAP and HE has achieved better...